SUMMARY:Fracture by a million impacts: Erosion of polycrystalline diamond 
 at temperatures up to 600 ˚C - Arthur Henderson\, SMF Group\, Cavendish L
 aboratory
DTSTART:20190314T160000Z
DTEND:20190314T170000Z
UID:TALK116062@talks.cam.ac.uk
CONTACT:Stephen Walley
DESCRIPTION:Polycrystalline diamond (PCD) was originally developed in the 
 1970s for use in tooling. During manufacture\, a transition metal catalyst
 \, usually cobalt\, is introduced to moderate the sintering pressures and 
 temperatures. However\, the cobalt binder remains within the PCD microstru
 cture and plays a key role in crack nucleation and propagation. Here\, the
  wear of PCD is studied using solid particle erosion at ambient and high t
 emperatures.